Effect of Nano-size Silicon Carbide (SiC) Reinforced Al 8088 Alloy in an Alkaline Medium using Static Immersion Method

Pruthviraj R D, Ashok S. D., Krupakara P. V., Jayasimha H. N.

Abstract


In this investigation, an strive has been made to broadenAl 8088reinforced with silicon carbide particulatenanocompositethrough liquid melt metallurgy method and to look at corrosion conduct.nanocomposite containing 2, 4 and 6 percent of SiC are preparedconsistent with ASTM requirements. Weight loss approach is carried out in 0.025N, 0.05N and 0.1N answers of KOH. The corrosion price decreases with boomin thepublicity time for all the specimens and decreases with the boom in reinforcement content material of thenanocomposites. Sincenanocomposites undergo much less corrosion compared to base alloy, which can be used for the manufacture of equipmentused in marine environment.

Keywords


nanocomposites, corrosion, Al 8088, silicon carbide, vortex

Full Text:

PDF

References


Abd Ei-Rehim SS, Ibrahim MAM, Khaled KF (1999) 4-Aminoantipyrine as an inhibitor of mild steel corrosion in HCl solution. J Appl Electrochem 29: 593–599.

Almeida E, Pereira D, Figueiredo MO, Lobo VMM, Morcillo M (1997) The influence of the interfacial conditions on rust conversion by phosphoric acid. Corros Sci 39: 1561–1570.

R Asthana, M Singh, N Sobczak (2005), The role of wetting and reactivity in infiltration of ceramic-metal composites, Ceram. Eng. Sci. Proc. 2,249–261.

Bellanger G, Rameau JJ (1996) Effect of slightly acid pH with or without chloride in radioactive water on the corrosion of maraging steel. J Nuclear Mat 228:24–37.

Bellanger G (1994) Effect of carbonate in slightly alkaline medium on the corrosion of maraging steel. J Nuclear Mat 217:187–193.

Cheng S, Chen S, Liu T, Chang X, Yin Y (2007) Carboxymethylchitosan + Cu2+ mixture as an inhibitor used for mild steel in 1 M HCL. Electrochim Acta 52: 5932–5938.

JECastle, LSun and HYan (1994). The use of scanning auger microscopy to locate cathodic centers in SiC/Al6061 MMC and to determine the current density at which they operate, Corrosion Science, 36(6), 1093–1110.

HE Deve, C McCullough (1995), Continuous-fiber reinforced Al composites: A new generation, JOM 4,33–37.

JMGDeSalazar, AUrefia, SMazanedo and MBarrens (1999), Corrosion behaviour of AA6061 and AA7075 reinforced with Al2O3 particulates in aerated 3.5%chloride solution potentiodynamic measurements and microstructure evaluation, Corrosion Science, 41, 529–545.

El-Neami KKH, Mohamed AK, Kenawy IM, Fouda AS (1995) Inhibition of the corrosion of iron by oxygen and nitrogen containing compounds. Monatsh Chem J 126: 369–376.

Gunasekaran G, Chauhan LR (2004) Eco friendly inhibitor for corrosion inhibition of mild steel in phosphoric acid medium. Electrochim Acta. 49: 4387- 4395.

GurrappaVV, Bhanu Prasad(2006)Corrosion characteristics of aluminium based metal matrix composites,Materials Science and Technology,22:1,115–22,DOI:10.1179/174328406X79324

KatsuakiSuganuma. (1993) Interfaces in β–SiC whiskers/6061 aluminum composites.Journal of Materials Research8:10, pages 2569–2576.


Refbacks

  • There are currently no refbacks.